Home | Forums | Register | Gallery | FAQ | Calendar |
Retailers | Community | News/Info | International Retailers | IRC | Today's Posts |
|
Thread Tools |
December 25th, 2009, 01:36 | #1 |
Holster wear on Slide
I know airsoft pistol finish arent made as good as firearms. How much wear will be shown from a Shooter Design's CNC slide from SERPA holster?
And which colour will show less wear? Black, Titanium, or Silver? (I wish it was stainless) |
|
December 25th, 2009, 01:41 | #2 |
What pistol?
With my USP, there was very little wear on the slide, it wasn't discolored or anything, but the black finish had turned a little less textured. That was after a year and a half of use though. On my MEU... well I haven't used it enough to notice a difference so far. |
|
December 25th, 2009, 03:35 | #3 |
so on USP I wouldnt expect the wear seen from Taiwanese or factory KSC metal slide right?
|
|
December 25th, 2009, 11:49 | #4 |
Official ASC Bladesmith
|
Likely it'd be a painted slide, so you might see wear marks (they look cool though), but on the Shooter's Design, I doubt it. I have the MK23 SD slide and it's anodized, which is a lot toughter than paint. But I can't comment on the holster in question since I don't own one, don't know where the wear marks occur from it (if any).
|
December 27th, 2009, 01:49 | #5 |
If you're a gamer and not a collector, why are you concerned?
Guns are meant to be used and have some wear on them! |
|
December 27th, 2009, 01:52 | #6 |
Factory slide will wear very badly, SD slide will not.
|
|
|
Bookmarks |
Thread Tools | |
|
|